MEMSnet Home: MEMS-Talk: Re: photoresist spinner
Re: photoresist spinner
1999-04-15
Kevin M Walsh
1999-04-15
jneogi
1999-04-15
Klaus Ruhmer at Home
1999-04-15
Jim Beall
1999-04-15
[email protected]
1999-04-16
Shile
Re: photoresist spinner
jneogi
1999-04-15
Winston:

We have been using the SCS Spin coater and it works great. I strongly
recommend the SCS spin coater and the price is great. They also have a
great leasing plan (~$500 for 3 months), you may lease it to check it
out.

Jayant
*****************************************
Jayant Neogi
Vice President & Chief Technical Officer
Ph#  503-640-0586
Fax  503-640-8117
http://www.norsam.com
*****************************************
Winston Chan wrote:
>
> Our photoresist spinner died last week and we are looking for a new one.
> I found several manufacturers of small benchtop spinners - Headway,
> Laurell, Cost Effective Equipment (part of Brewer Science) and SCS
> (Specialty Coating System). Does anyone have experience, good or bad,
> with these spinners? Are there others that I should be looking into?
>
> Winston
>
> --
> Winston Chan                            | phone: (319) 353-2398
> Dept. of Electrical Engineering         | fax: (319) 353-1115
> University of Iowa                      | email: [email protected]
> Iowa City, IA 52242
>

--


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Nano-Master, Inc.
Addison Engineering
Process Variations in Microsystems Manufacturing