Re: Dicing into circular quartz dice
Jayant Neogi
1999-04-27
You can use an Ultra sonic cutter to precisely cut 10mm circular disk and
this technique works great. Folks have been using this technique to generate
TEM samples. If you want to keep the dies together you can bond the glass
substrate to a thick resist sheet and after the dicing process dissolve the
resist in acetone. Let me know if you have any other questions.

Jayant
*************************************************
Jayant Neogi
Vice President & Chief Technical Officer
Norsam Technologies Inc.
Ph# (503) 640-0586
Fax  (503) 640-8117
http://www.norsam.com
*************************************************
-----Original Message-----
From: John D. Evans 
To: [email protected] 
Date: Tuesday, April 27, 1999 1:08 AM
Subject: Dicing into circular quartz dice


>
>MEMS Community,
>
>I am interested in dicing up a 500 um quartz wafer into circular dice,
>roughly 10 mm diameter. I have two questions:
>
>1) What technologies and companies are available to do the cutting
>(preferably in California)?
>
>2) How do you hold the wafer and dice during cutting? If you hold the wafer
>only, then the circular parts will fall into the cutting stream/beam and
>get damaged. Is there a way to hold the individual dice? Is there a
>substrate that doesn't get cut that you can "glue" to both the wafer and
dice?
>
>Any suggestions appreciated.
>
>Thanks,
>
>John D. Evans
>Silicon Waterworks
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Addison Engineering
MEMS Technology Review
Mentor Graphics Corporation