MEMSnet Home: MEMS-Talk: Re: LPCVD nitride wafers
Re: LPCVD nitride wafers
1999-04-26
Roger Neef
Re: LPCVD nitride wafers
Roger Neef
1999-04-26
Hello Kevin,

My name is Roger Neef and I am with a company called Silicon Valley
Microelectronics.  We are a supplier of Si wafers as well as films and
services.  If you would like to contact me at the number below I would be
happy to take your specifications and offer you a competitive quotation.

Best regards,










At 11:34 PM 4/21/99 -0400, Kevin M Walsh wrote:
>
>I wish to purchase (100) silicon wafers with low stress nitride.
>Can anyone provide source info?
>
>--
>Dr. Kevin M. Walsh
>Electrical Engineering Department, Speed Scientific School
>University of Louisville, Louisville, KY 40292
>(502) 852-0826
>
>Internet address: [email protected]
>
>
>
Roger Neef
Silicon Valley Microelectronics, Inc.
North America Wafer Division
Tel: 408-436-2351
Fax: 408-436-8402
WWW.SVMI.COM


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation