Al2O3 etchant
1999-12-09
alexander chimbayo
Al2O3 etchant
alexander chimbayo
1999-12-09
Could anyone let me know an etchant I can use to remove Alumina (Al203)
film on glass that would not attack the glass ?
Thanks,

Alexander