Dear MEMS collegues:

I am working on the laser forming  of metals, using laser to scan the
material to introduce
thermal stress in the material. It is very important to have the flow
stress datas, to
1. Improve of the design
2. Diagnostics during the manufacturing:
3. have better undertsnading of the material's microstructure change
during the manufacturing.

The temperature in the scanning path is in range of 400C---1500C,  flow
stress is in the range of
200MPa to 400MPa.

I am looking for some coorperation. Does anyone know the publications or
web adresses to extract these
informations ?
Thank you very match;
Best regards

George Cheng

Manufacturing Research Labortory
Columbia University
New York NY,10027
(o): (212)666-2393


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Addison Engineering