MEMSnet Home: MEMS-Talk: all-dry lithographic process
all-dry lithographic process
2000-01-06
Murat GEL
all-dry lithographic process
Murat GEL
2000-01-06
Is there anyone who knows about all-dry lithographic process?
ex: DESIRE process (Dry etching of Silylated Image Resist)
or SAHR process (silylated acid hardened resist)

I am trying to buy that kind of a resist. Anyone doing similiar dry
lithography ? Any piece of information would be very appreciated.
Thankyou.
Murat GEL