Dear Colleagues,
We are metallizing copper plated PCB's. Does anyone know if there is a
preferred surface depassivation and activation procedure?  Copper is
generally not catalytic to electroless metallization.  Hope everyone is
enjoying their summer. Thanks as always for the help.
Cheers,

Cindi Prorok
Argonide Nanomaterials Group
[email protected]
www.argonide.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Harrick Plasma, Inc.
Mentor Graphics Corporation
MEMS Technology Review