Nickolay,

The best resource for linear solutions to plate problems is

Roark's Formulas for Stress and Strain
By Warren C. Young
McGraw-Hill Inc.
ISBM 0-07-072541-1


Best Regards,

Loren St. Clair

EV Group-Technology, Tel: (602) 437 9492 x 109, Fax: (602) 437 9435
E-mail: [email protected]  , Web:
www.EVGroup.com  , Date: 9/22/2000



                -----Original Message-----
                From:   Nickolay Lavrik [mailto:[email protected]]
                Sent:   Thursday, September 14, 2000 12:55 PM
                To:     [email protected]
                Subject:        Q:spring constant calculation

                Does anyone know the equation (or the reference where it can
be found)
                that can be used to estimate a spring constant of a thin
plate (such as
                microcantilever) based on the plate geometry (thickness,
width, length)
                and Young's modulus of the material ?


                You help will be much appreciated.


                --
                Nickolay Lavrik
                University of Tennessee
                Department of Chemistry
                420 Buehler Hall

                Ph.(865) 974-6174


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
MEMS Technology Review