MEMSnet Home: MEMS-Talk: patterning of rustless foil
patterning of rustless foil
2000-10-26
Ivan Kostic
patterning of rustless foil
Ivan Kostic
2000-10-26
Dear colleaques,

we are looking for any advice which is the most simpliest
high throughput  method for
fabrication of large structures in a rustless foil.
Foil thickness of about 50 micron, patterns with a minimal
rustless linewidth
of about 30 micron over a few square centimeters large area.

Any response is highly appreciated.

Best regards,
Ivan Kostic





________II SAS________________________________
Laboratory of E-Beam Lithography and Microstructuring
Tel. +421-7-5941-2006,-2557   Fax: +421-7-5477-1004
http://ups.savba.sk/ebl _____________Bratislava_____


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
University Wafer
Mentor Graphics Corporation