Re: SU-8
2000-11-27
Kien Choon Wong
2000-12-04
Christopher Levey
Re: SU-8
Kien Choon Wong
2000-11-27
Dear MEMS specialists,

I would like to know what method is best for getting the same amount of SU-8
onto the glass substrate each time rather than estimating the amount. At this
moment, I used a plastic stick to scoop SU-8 onto the glass. Also, I have
tried using pipettes but failed because SU-8 is too thick. Please help.
Thanks.

regards,

Kien

Kien Choon Wong
University of Birmingham
EMD Group
Edgbaston
Birmingham, UK

____________________________________________________________________
Get free email and a permanent address at http://www.amexmail.com/?A=1


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing