li shifeng
ask help about KOH etch
li shifeng
2000-11-30
sir,
I read your post from cleaning house.According to your recipe, i did KOH
etch experiment.but the result is much different.the etch rate is just 15
micron/hour.My case is the following
N type 3" wafer
250ml water
63ml isopropyl alcohol
57.9g 89.7% KOH
Temperature of soluation was maintained at 80 degree celsius.

would you like give me some suggestions? thanks

________________________________________________________________________________
_____
Get more from the Web.  FREE MSN Explorer download : http://explorer.msn.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
University Wafer
Tanner EDA by Mentor Graphics
The Branford Group