MEMSnet Home: MEMS-Talk: Re: Si wafer facilities for microsystem fabrication
Re: Si wafer facilities for microsystem fabrication
2001-02-26
Bernard Courtois
Re: Si wafer facilities for microsystem fabrication
Bernard Courtois
2001-02-26
Dear Andreas,

This is in addition to the reply by Gerold Schröpfer.

At CMP, we run 6'' wafers for microsystems (http://cmp.imag.fr).

Regards,

Bernard COURTOIS

Gerold Schröpfer wrote:

> Hello Andreas,
>
> Most of the European foundries are still running 4" wafers and many are
> planning not to switch to 6" until they are forced through supply of
> equipment for 4" etc.
>
> To my knowledge the following European foundries handle 6" Si wafers:
>
> -BOSCH - Reutlingen, Germany
> -Colibrys - Neuchatel, Switzerland (foundry spin off from CSEM in January
> 2001)
> -FhG ISiT - Itzehoe, Germany
> -OnStream, Holland
> -ST, Italy
> and X-Fab in Erfurt that you certainly know well
>
> There are relatively more in the US the offer 6" wafer capacities.
> Unfortunately, almost all of them will not be interested in small volumes
> (however it is not always the volume that counts). To my knowledge most R&D
> institutions do not offer 6" wafer runs, but generally 4".
>
> One possibility might be the CMI at the EPFL in Lausanne. They have really
> 'nice' cleanroom facilities running on 6". You may contact Prof. Philippe
> Renaud ([email protected]).
>
> If you need more information, your are welcome to contact me.
>
> Best regards
> Gerold
>
> ----
> Dr. Gerold Schrvpfer
> Foundry Program Manager
>
> COVENTOR Sarl
> 3 Avenue du Quebec
> ZI de Courtaboeuf
> 91140 Villebon sur Yvette
> France
>
> Tel: +33 (0)1 69 29 84 85
> Fax: +33 (0)1 69 29 84 88
> Mobile: +33 (0)6 75 01 43 57
>
> COVENTOR: http://www.coventor.com
> -----Original Message-----
> From: Andreas Albrecht [mailto:[email protected]]
> Sent: Friday, February 16, 2001 5:58 PM
> To: [email protected]
> Subject: Si wafer facilities for microsystem fabrication
>
> Dear colleagues
> who knows Si wafer manufacturing facilities in R&D institutes (because
> of small to medium volume production) prefered in Germany and could tell
> me which
> wafer sizes are processed there.
>
> There is an urgent need for 6" wafer foundry processes.
>
> Regards
> Andreas Albrecht
>
> Transferzentrum Mikroelektronik e.V.
> In den Weiden 7
> D-99099 Erfurt
> Tel. +49-(0)361-42051-75        Fax +49-(0)361-42051-76

--
Bernard Courtois TIMA-CMP   Tel: +33 4 76 57 46 15
46 avenue Felix Viallet     Fax: +33 4 76 47 38 14
38031 Grenoble Cedex-FRANCE Email: [email protected]
http://tima.imag.fr


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Nano-Master, Inc.
The Branford Group