MEMSnet Home: MEMS-Talk: AZ 1505 photoresist
AZ 1505 photoresist
2001-03-01
Beatriz Palacios
AZ 1505 photoresist
Beatriz Palacios
2001-03-01
We have seen that you are working in microelectromechanical system and we
would appreciate  any information about the following related question.

We are developing AZ 1505 photoresis with AZ 351 developer, that is a 0.5 %
Sodium hidroxide solution. We would like to know if it is possible to
prolong the lifetime of our developer and how.

We look forward to hearing from you soon.


Beatriz Palacios


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Harrick Plasma, Inc.