A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Re: SOI (111) Cnrs- Fr
Re: SOI (111) Cnrs- Fr
2001-03-19
Kenneth Smith
Re: SOI (111) Cnrs- Fr
Kenneth Smith
2001-03-19
I don't know why Soitec does not provide this as it is simply a different
base wafer that is processed prior to the bonding.
I you are still interested in the 1-1-1, please send me you complete
specification, including bond oxide thickness, top and base wafer
specifications including dopant, resistivity, orientation needs, Thickness
( handle and device).
I can supply virtually any silicon wafer that you might need with TTV < 1
um in DSP and can also arrange for the bonding , thinning and final polish.

Best Regards,
Ken Smith
Kmbh Associates
4968 Charter Road
Rocklin, CA  95765  USA
510-714-5055 Efax- 510 217 4421 or 561 658 6136

High Purity Float Zone and Specialty CZ Silicon  for Power, IR and Mirror
Optics, Optoelectronics, MEMS, SOI, and other Semiconductor applications.
Service in SOI, Polishing SSP and DSP

David Peyrade wrote:

> Dear MEMs researchers,
>
> I am interested in SOI wafer but with Si (111).
> SOITEC does not make this kind of product.
> Do you know another company or a research laboratory who sells SOI(111)
> ?
>
> Yours sincerely
>
> ------------------
> David Peyrade
> Ph.D. Student
> L2M-CNRS
> 196 Av. H. Ravera
> 922225 Bagneux
> FRANCE
>
> Tel: 01 42 31 73 74
> Fax: 01 42 31 73 78

.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation