2000-01-24
Shay Kaplan
2001-04-11
Weijie Wang
Black Wax
Weijie Wang
2001-04-11
Hello,

I am going to use black wax to protect the backside of Si during KOH
etching. I was told that black wax can be spin-coated on Si when it is
dissoved in certain organic solvent. Does anyone know which solvent is the
best candidate for this work? What is the ratio of wax and solvent?
How to bake the film after spin-coating?
Thank you in advance.

Weijie Wang


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics