MEMSnet Home: MEMS-Talk: Photodefinable polyimide
Photodefinable polyimide
2001-05-13
Yiping Lin
Photodefinable polyimide
Yiping Lin
2001-05-13
Hi:

I look for solution about insulating layer. Using phtodefinable polyimide is one
possibility and can reduce the steps of processing. However, I had bad
experience with spin-on glasses on cuing temerature, and polyimide also needs to
be cure at several temperatures. Do you have experiences with using polyimide as
insulating layer? If you like to share with me, please send an email to

[email protected]

Thanks.

Yiping Lin
Department of Physics and Astronomy
SUNY at Stony Brook, Stony Brook, NY 11794-3800
__________________________________________________________________
Get your own FREE, personal Netscape Webmail account today at
http://webmail.netscape.com/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation