Dr. Ildiko Tanczos
2001-02-15
Hi, we have worked a lot with TMAH, but we do not know about a reaction
of TMAH with Au.

I. Tanczos

----- Original Message -----
From: 
To: ; ; ;
; ;
; ;
; 
Cc: ; 
Sent: Thursday, February 08, 2001 10:53 AM
Subject: From HKUST


>
> Hi, this is xu wehua,from Hong Kong Science and
> Technology.
>
> WOuld you please tell me if TMAH and Au have a
> reaction?? If have a reaction,what is the
> reaction rate??
>
> Does any one know if gold is etched by TMAH ??
>
> Regards,
>
> Xu Weihua
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Harrick Plasma, Inc.
MEMStaff Inc.
Process Variations in Microsystems Manufacturing