MEMSnet Home: MEMS-Talk: SU-8 molds on glass substrate
SU-8 molds on glass substrate
2001-08-01
Ashish Singh
SU-8 molds on glass substrate
Ashish Singh
2001-08-01
Dear all,

I am working on a process for making SU-8(stvn-2) molds on glass substrate. I am
facing a problem
that the SU-8 mold starts peeling off from the glass substrate after a period of
about 1 day.

Looking at the nature of the problem, my guess is that it can be either due to
lack of adhesion
between SU-8 and glass or it may be due to development of internal stresses.

If you have any ideas about how to eliminate these problems, kindly give me your
suggestions.

Thanks in advance
Regards

Ashish Singh
Graduate Student
Rochester Institute of Technology


__________________________________________________
Do You Yahoo!?
Make international calls for as low as $.04/minute with Yahoo! Messenger
http://phonecard.yahoo.com/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMStaff Inc.
The Branford Group
Harrick Plasma, Inc.