MEMSnet Home: MEMS-Talk: TMAH
TMAH
2001-08-08
ÂÞÔª
2001-08-08
Anthony Flannery
TMAH
Anthony Flannery
2001-08-08
Add a small amount of ammonium persulfate. This technique was published
by Erno Klaussen at Stanford.

ÂÞÔª wrote:

> Dear Sirs:
>     We want to etch a V-groove with TMAH.But our experiments showed
> that the surface is very rough with many hilllocks. By add IPA or
> (NH4)2S2O3, the surface is still rough.And the concentration of the
> TMAH we used is 5%(wt)~22%(wt).
>     Would someone kindly to tell us how to have a V-groove without
> hilllocks by using TMAH?
>     Thanks a lot.
>
>     Best Regards!
>
>                        Yours Sincerely:LuoYuan
>                            Aug.8,2001
>
> _______________________________________________
> mems-talk mailing list
> [email protected]
> http://fab.mems-exchange.org/mailman/listinfo/mems-talk



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Nano-Master, Inc.