Etching InGaP and GaP
2001-08-21
Rozenn Keravec
2001-08-22
oray orkun cellek
Etching InGaP and GaP
oray orkun cellek
2001-08-22
1 Bromine: 100 DIW solution would etch non selectively.  That was once used
for <1um deep mesa etching of GaInP/InGaAs/GaAs for 20sec. .  I do not know
the etch rate.