DRIE
2001-09-04
Helen Berney
2001-09-04
Sonbol Massoud-Ansari
DRIE
Sonbol Massoud-Ansari
2001-09-04
Dear Dr. Berney,

We provide DRIE of 4" silicon wafers at ISSYS.  Please feel free to contact
me and I'd be happy to discuss your process requirements.

Best Regards,

Sonbol Ansari

--

*******************************
Sonbol Massoud-Ansari
Director of External Services
Integrated Sensing Systems, Inc.
387 Airport Industrial Drive
Ypsilanti, MI 48198
Tel : (734) 547-9896 ext. 104
Fax : (734) 547-9964
Email : [email protected]
WWW : http://www.mems-issys.com
*******************************


Helen Berney wrote:

> Hi all,
>
> I am looking for a foundry that can perform deep reactive ion etching
> (375 micron etch in 525 or 750 micron silicon wafers).  Ideally I am
> looking for somewhere that can process four inch wafers.  Depending on
> clean room constraints, I can supply patterned nitride on silicon wafers
> for further processing or discuss our full process requirements with the
> relevant fab.  Initially I am looking for a smalll number of wafers
> (5-10) to prove a concept.
>
> thanks,
>
> Dr. Helen Berney
> National Microelectronics Research Centre, LeeMaltings,Cork, Ireland.
> Tel +353-21-4904010 Fax +353-21-4270271 Email [email protected]
>
> _______________________________________________
> mems-talk mailing list
> [email protected]
> To unsubscribe or change your list options, use:
>  http://fab.mems-exchange.org/mailman/listinfo/mems-talk





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics