InP CTE for temperature range of 50C to 250C
2001-09-18
Randall Cha (Dr)
2001-09-20
oray orkun cellek
InP CTE for temperature range of 50C to 250C
Randall Cha (Dr)
2001-09-18
Dear colleagues,

I will very much like to know the coefficient of thermal expansion (CTE)
of InP from 50C to 250C. Any valuable inputs from all?

Many thanks in advance.

Best rgds,
Randall
Principal Engineer,
DLS, Singapore
Tel : 65-4154447
Fax: 65-4154444



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
The Branford Group
Process Variations in Microsystems Manufacturing