Dear MEMS colleagues,
        I have two questions Related two the use of TMAH:

1) What percentage of Si or Al, (or solution),  in TMAH would suppress
Aluminium or Cr etching.
2) Has anyone, encountered any problems with etching polycrystalline silicon
(100), taking
into account there is no oxide present - this has just happen to me all of a
sudden.

-->some other matrial on top or change in orientation of poly - wild guess?

any suggestion with regards to 2) will be much appreciated!!!!

thank you for your interest,

Philip Lau


********************************************************************
This email and any attachments are confidential to the intended
recipient and may also be privileged. If you are not the intended
recipient please delete it from your system and notify the sender.
You should not copy it or use it for any purpose nor disclose or
distribute its contents to any other person.
********************************************************************


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Harrick Plasma, Inc.