Dear members:

We are trying to make an ultrasonic transducer using PZT as the piezoelectric
material. If anyone happens to know the etching techniques of PZT as well as
the adhesion techniques of PZT to Si substrate, please give some suggestion.
Any resource of publications on these issues is also urgently needed.

Thank you very much.

Yours sincerely,

Qun LI
Dept. of Biomedical Engineering
Louisiana Tech University
Ruston, LA 71272


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
University Wafer
MEMS Technology Review
Process Variations in Microsystems Manufacturing