XeF2 on 4" wafers
1996-05-30
Tom Rust
XeF2 on 4" wafers
Tom Rust
1996-05-30
We also tried XeF2 at UCLA on a 4" wafer. Their system has control over etch
rate either in regulated volumes released into the reaction chamber or as a
continuous flow. I didn't find much difference. The range was also around .1-.2
u/min. We also tried placing an oxide coated wafer next to the backside to
reduce the loading, but it didn't have a noticable effect. The only strange
thing I noticed was a fine black powder which appeared around the edge of the
wafer. ??? Otherwise, there was no appreciable etching of resist,
oxide,nitride, or the metals we used other than the Si.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
MEMS Technology Review
Process Variations in Microsystems Manufacturing