MEMSnet Home: MEMS-Talk: Ablation
etching selectivity between Cr and Ag
Re: Diffusivity and Solubility of metals in Silicon
2001-10-03
Craig McGray
Re: Electric breakdown in MEMS air gap
2001-10-03
Craig McGray
2001-10-03
David Yen
Processing equipment
2001-10-03
Inna Mushkatinskaya
Ablation
2001-10-03
Inna Mushkatinskaya
RE: mems-talk digest, Vol 1 #61 - 8 msgs
2001-10-03
Pancham R. Patel
Ablation
Inna Mushkatinskaya
2001-10-03
Hello,

Does anybody know of good source of information on excimer laser ablation
of inorganic materials? I'm sure that there are fundamental hand-books
about it, other than Duley "UV lasers: effects and applications in material
science".

Thanks a lot for all of your help,

Inna.

[demime 0.98e removed an attachment of type text/x-vcard which had a name of
innam.vcf]

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Addison Engineering
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.