photoresist bonding
Jianzhong Zhu
2001-11-01
Dear Reni,

Thanks for you answer to my question. We do want to
use dry film photoresist for PCB. May I ask another
question: can we bond a fresh photoresist onto a
developed one?

Thanks,
Jianzhong

--- Reni Fliron  wrote:
> If you are using dry film photoresist for PCB
> fabrication, it is my experience that:
> -It bonds poorly to silicon oxide
> -It bonds to silicon, low res. can be difficult
> -The best result is obtained with a thin
> metal layer on the wafer.
>
> Reni Fliron
>
> -----Original Message-----
> From: Jianzhong Zhu [mailto:[email protected]]
> Sent: 31. oktober 2001 16:54
> To: [email protected]
> Subject: [mems-talk] photoresist bonding
>
>
> Hi, All,
>
> Is there any body have experience to bond dry film
> photoresist onto silicon wafer? We hope to bond them
> directly, if possible.
>
> Thanks,
> Jianzhong
> Make a great connection at Yahoo! Personals.
> http://personals.yahoo.com
> _______________________________________________
> mems-talk mailing list
> [email protected]
> To unsubscribe or change your list options, use:
>
http://fab.mems-exchange.org/mailman/listinfo/mems-talk
Make a great connection at Yahoo! Personals.
http://personals.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
Process Variations in Microsystems Manufacturing
Addison Engineering