A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: ion imlant depth vs energy for As, B, etc
photoresist heat capacity
2001-11-05
Andrey Bayrashev
ion imlant depth vs energy for As, B, etc
2001-11-06
jaideep mavoori
2001-11-08
Sonia Garcia Blanco
ion imlant depth vs energy for As, B, etc
jaideep mavoori
2001-11-06
Hello.
Is there a table/software for calculating ion implant depth vs energy for
various tilt angles for various species and substrates (Si primarily).

Thanks.
Jaideep

reply