A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: ion imlant depth vs energy for As, B, etc
ion imlant depth vs energy for As, B, etc
2001-11-08
Jaideep Mavoori
2001-11-09
Burkhard Volland
ion imlant depth vs energy for As, B, etc
Jaideep Mavoori
2001-11-08
Others have indicated interest in this data and hence I am posting this for
the group.  Thanks to Michael Yakimov, for the following link.  I found it
helpful.
http://www.research.ibm.com/ionbeams/SRIM/SRIMLEGL.HTM

Thanks also for the other pointers I received, like this from Mehmet
Dokmeci:
"A year ago I had the same question and the ion implant company,
IICO and as well as the other one implant sciences do have
these tables and will fax them to you if you contact them.
Good luck,

-Mehmet"

Thanks one and all.
Jaideep

----- Original Message -----
From: "Michael Yakimov" 
To: "jaideep mavoori" 
Sent: Wednesday, November 07, 2001 7:03 AM
Subject: RE: [mems-talk] ion imlant depth vs energy for As, B, etc


> SRIM
> http://www.research.ibm.com/ionbeams/SRIM/SRIMLEGL.HTM
>
>
> > -----Original Message-----
> > From: jaideep mavoori [SMTP:[email protected]]
> > Sent: Tuesday, November 06, 2001 12:46 AM
> > To: [email protected]
> > Subject: [mems-talk] ion imlant depth vs energy for As, B, etc
> >
> > Hello.
> > Is there a table/software for calculating ion implant depth vs energy
for
> > various tilt angles for various species and substrates (Si primarily).
> >
> > Thanks.
> > Jaideep
> > _______________________________________________
> > [email protected] mailing list: to unsubscribe or change your list
> > options, visit http://fab.mems-exchange.org/mailman/listinfo/mems-talk
> > Hosted by the MEMS Exchange, providers of MEMS processing services.
> > Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Addison Engineering
Mentor Graphics Corporation