MEMSnet Home: MEMS-Talk: WETTING AGENTS
WETTING AGENTS
1996-06-11
Michael Young
WETTING AGENTS
Michael Young
1996-06-11
Dear MEMS,
I am currently having problems electroplating small nickel features (typically
a few microns) through thick photoresist. I am unable to get the electroplating
solution (Nickel sulphate based) into all the resist openings due to the high
aspect ratios and small dimensions. I would be grateful if anyone could suggest
a suitable wetting agent to overcome this problem.

Cheers,
Mike Young.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
Mentor Graphics Corporation
MEMS Technology Review