MEMSnet Home: MEMS-Talk: Planarization
Planarization
2001-11-16
Ajey P. J.
Ag RIE
2001-11-20
Qingwei Mo
Planarization
Ajey P. J.
2001-11-16
Hello,

I have to put Al contacts on a Si mesa structure which is of 1.3 um in
height. I would like to do planarisation on the substrate (Si) with respect
to the mesa structure such that i could reduce the height. Can any one
suggest me how to do the planarization and the right polymer to be used for
this.

                     _________
              ____Al______    |
             |            |   |
             |            |1.3| um
             |            |___|______
    _________|            |____Al_____
                      Substrate
  ____________________________________


Thanking you all in advance,

Ajey Jacob.



_________________________________________________________________
Get your FREE download of MSN Explorer at http://explorer.msn.com/intl.asp

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Nano-Master, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics