Dear all:

I am now doing an experiment which need to etch the silicon without attacking
Al. The alkaline etchants that we usually adopted in MEMS, TMAH and KOH, could
not satisfy the requirement. I heard that some organic material can do this job,
can anyone here provide me the information? Or advise me other effective
solutions? Anything you provided will be highly appreciated!

Thanks

Daniel

************************************************************
Daniel Xu (Xu zhengyi)
------------------------------------------------------------
Ph.D candidate
State Key Laboratories of Transducer Technology
Shanghai Institute of Microsystem & Information Technology
Chinese Academy of Sciences
865 Changning Road
Shanghai 200050
China
------------------------------------------------------------
Tel: 86-21-62511070 ext. 8607
FAX: 86-21-62513510
email:[email protected]
************************************************************

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
MEMS Technology Review
Mentor Graphics Corporation