MEMSnet Home: MEMS-Talk: wire bonding on Ti Au
wire bonding on Ti Au
2001-12-05
Satej Chaudhary
2001-12-08
Yahong Yao
wire bonding on Ti Au
Satej Chaudhary
2001-12-05
> Hi,
>
> I would like to know what is the minimum thickness
> of the upper gold layer on a
> Ti/Au pad in order to proceed to a wire bonding
> without any risk?

0.5 microns is the standard way to go i have heard
though i havnt tried it myself.
satej
Grad student University of Maryland
Send your FREE holiday greetings online!
http://greetings.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Mentor Graphics Corporation
Addison Engineering