In our ICP, we are not allowed to use metal masks. I heard that once a guy
used a metal mask, it cost a LOT to get the piece of equipment fixed.

Sun

At 04:18 PM 12/7/01 +0100, you wrote:
>Hello,
>
>I know that with Alcatel DRIE engines we can use Al as mask can we do it
>with STS multiplex ICP too ?
>
>Thanks for yoour help
>
>Matthieu
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
The Branford Group
MEMS Technology Review