MEMSnet Home: MEMS-Talk: plasma chemistry for E-glass etching
plasma chemistry for E-glass etching
2001-12-07
Robert Dean
2001-12-07
martin.walker4
2001-12-07
[email protected]
2001-12-08
[email protected]
2001-12-11
Jon Doe
any hydrophillic layer?
2001-12-11
jung hoon yeom
2001-12-12
Helen Berney
2001-12-11
[email protected]
plasma chemistry for E-glass etching
martin.walker4
2001-12-07
Your question is a good one.  Many people assume that 'glass' is as easy to
etch as SiO2, but it just is not so!  Fluorine chemistry will remove SiO2
(e.g. CF4, CHF3, C4F8) but will not touch Al2O3.  You need chlorine and/or
Bromine in there in some form too.  It has been done using CF3Cl, but this
is a CFC which is either banned or about to be.  Try running something like
a mix of CF4 and Cl2 if your chamber is load-locked, or you have a glove
box.  If you don't, avoid Cl2 as you are likely to get a very nasty smell
when you open the chamber.  Other possible gases include BCl3, HBr and
SiCl4, but all these are toxic and corrosive, so need to be treated with
caution.  This area is beginning to develop.  Keep in touch with the various
manufacturers (see the equipment list on
http://www.e-insite.net/semiconductor/index.asp?layout=buyersGuideSearch)
and look for new data sheets relating to this.

Regards,

Martin Walker, Tactical Marketing Engineer, Oxford Instruments Plasma
Technology
(www.oxford-instruments.com/plmchp5.htm)
----- Original Message -----
From: "Robert Dean" 
To: 
Sent: Friday, December 07, 2001 4:00 PM
Subject: [mems-talk] plasma chemistry for E-glass etching


> Hello,
>
> I am looking for a plasma chemistry for RIE etching E-glass, which is
> composed of silicon dioxide, calcium oxide, aluminum oxide, boron oxide,
> and trace amounts of sodium, potassium and magnesium oxides.  Silicon
> dioxide is not a problem to RIE etch.  Thanks.
>
> Sincerely,
>
>
> Robert Dean
>
> Research Associate IV
> Center for Advanced Vehicle Electronics
> Auburn University
> 200 Broun Hall
> Auburn, AL 36849
>
> Voice: 334-844-1838
> Fax:   334-844-1898
> Email: [email protected]
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
The Branford Group