MEMSnet Home: MEMS-Talk: More safety Porous Silicon process
More safety Porous Silicon process
2001-12-09
Luiz Marangoni
2001-12-10
Hawkins, Jeff
2001-12-11
Luiz Marangoni
2001-12-10
[email protected]
More safety Porous Silicon process
Luiz Marangoni
2001-12-11
Hello Jeff,

First of all, thank you for your answer. Could you give me more details
about the process?

Thank you very much

luiz marangoni
[email protected]



>Luiz,
>I have done some work with porous silicon in HNO3....
>
>
>
>-----Original Message-----
>From: Luiz Marangoni [mailto:[email protected]]
>Sent: Sunday, December 09, 2001 5:10 PM
>To: MEMS Talk List
>Subject: [mems-talk] More safety Porous Silicon process
>
>
>Hello group,
>
>I4m beginning a phD research about porous silicon. The first step of my
>study is  to develop a reactor to get macroporous silicon by anodical
>etching in a reliable way. A preliminary bibliographic seek about this
>item  revealed that the more commonly used etchant is the hydrofluoric acid
>(HF). I think all you know how dangerous is to work with HF, a highly
>corrosive compound. My inquiry to the group is if someone know other
>etchant that enables a more safety and a less hazardous process to get
>porous silicon. (I found something about ammonium fluoride...).
>I4m looking for people that have interest in form a research group about
>this subject. Someone have interest?
>
>Thank you
>
>
>Luiz Marangoni
>MEMS Enginneering Phd. Student
>State University of Campinas - UNICAMP - Brazil
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.mems-exchange.org/
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.mems-exchange.org/
>
>
>
>---
>Incoming mail is certified Virus Free.
>Checked by AVG anti-virus system (http://www.grisoft.com).
>Version: 6.0.303 / Virus Database: 164 - Release Date: 24/11/01

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation