A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: any hydrophillic layer?
any hydrophillic layer?
2001-12-11
[email protected]
2001-12-12
Helen Berney
2001-12-12
Liz Shelley
2001-12-12
Islam Rafiqul
any hydrophillic layer?
Islam Rafiqul
2001-12-12
If you do reverse RCA clean (no HF dip) on native oxide, it will make your
surface hydrophilic...

Best Regards,
Rafiqul Islam


EV Group Inc.- Technology- Tel: (602) 437 9492 x 118, (602)2842134
(cell),Fax: (602) 437 9435,
e-mail: [email protected] web: www.EVGroup.com


-----Original Message-----
From: Liz Shelley [mailto:[email protected]]
Sent: Wednesday, December 12, 2001 5:47 AM
To: [email protected]
Subject: Re: [mems-talk] any hydrophillic layer?


How thick a coating is necessary?
Any method of growing (even a native oxide) on silicon will cause the
surface to become hydrophillic.  H2O2 exposure will do.

> From: jung hoon yeom 
> Reply-To: [email protected]
> Date: Tue, 11 Dec 2001 15:11:59 -0600 (CST)
> To: 
> Subject: [mems-talk] any hydrophillic layer?
>
> Dear folks in the mems community
>
> I'd like to do conformal deposition on the Si substrate and modify it to
> hydrophillic surface(not hydrophobic) regardless of its thickness. And I
> am open to any kind of pocessing.
>
> Thanks
>
> Junghoon Yeom   University of Illinois at Urbana-Champaign
> Research Assistant  Department of Mechanical & Industrial Engr
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search