Hello,

I deposited SiN on fully cured polyimid (@350C) using PECVD at 250.
Polyimid will be removed to release nitride membrane. However,
I found the cracking of the nitride film. Our PECVD nitride film has
fairly low tensile stress ~150Mpa. So, is the cracking due to the CTE
mismatch between SiN and polyimid?  Has anyone done similar experiments?

Thanks
____________________________________________________________________
Kyu-Tae Yoo
Ph.D. candidate

Cornell University                       Phone:530-752-2522(office)
#117 Phillips Hall                            :530-902-5153(cell)
Computer and Electrical Engineering           :530-297-5153(Home)
Ithaca, NY  14853-5401                   eFax :509-463-1127

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Addison Engineering