MEMSnet Home: MEMS-Talk: bonding silicone rubber or PMMA with Si or poly-S i
bonding silicone rubber or PMMA with Si or poly-S i
2001-12-12
[email protected]
2001-12-13
Skrobis, Kenneth
bonding silicone rubber or PMMA with Si or poly-S i
[email protected]
2001-12-12
RTVs (room-temperature-vulcanizing silicones) are commonly used
for silicon chips that are sensitive to packaging stress, such as pressure
sensors.
GE makes a line of these for various other applications,
but they are well-suited for silicon, silicon dioxide, and gold as well.

-----Original Message-----
From: Ebin Liao [mailto:[email protected]]
Sent: Tuesday, December 11, 2001 8:50 PM
To: [email protected]
Subject: [mems-talk] bonding silicone rubber or PMMA with Si or poly-Si


Dear All:

I have made a micromachined sensor chip, and now I'd
like to bond it (Si or Poly-Si) to some polymeric
slices (silicone rubber or PMMA). Someone told me it
was very difficult to bond silicone rubber with other
materials. Anyone has experience for bonding silicone
rubber or PMMA to Si or poly-Si? I'd like to try Super
Glue by hand at first. Anyone has other suggestions?
Thanks a lot.

Best regards,

Ebin
Check out Yahoo! Shopping and Yahoo! Auctions for all of
your unique holiday gifts! Buy at http://shopping.yahoo.com
or bid at http://auctions.yahoo.com
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
MEMStaff Inc.
University Wafer