2001-12-14
Lior Grossman
2001-12-14
Mighty Platypus
2001-12-14
Erol Harvey
2001-12-16
Glenn West
2001-12-14
Alex Pozdin
Laser Ablation
Mighty Platypus
2001-12-14
From checking google [laser ablation mems], I came up with  the Short
Pulse Laser Ablation Technologies Laboratories (SPLAT) at UIUC. Below are
a couple of theiur publications. This should help, I think.

Li, C. and M. A. Shannon, "A Simplified Cavity Analysis for Estimating
Energy Coupling during Laser Ablation and Drilling of Solids -
Experiment," Applied Surface Science, 150, 211-226, 1999.

Shannon, M. A., "A Simplified Cavity Analysis for Estimating Energy
Coupling During Laser Ablation and Drilling of Solids - Theory," Applied
Surface Science, 127-9, 218-225, 1998.



Jesse Fowler
  UCLA/MAE Dept., 420 Westwood Plaza, Room 18-121, ENGR IV
  Los Angeles, CA 90095-1597 | (310)825-3977
"Rule #6: There is no rule #6" -- Monty Python
"ARTICLE SIX:  THIS ARTICLE IS ABOLISHED" -- Constitution of Afghanistan

On Fri, 14 Dec 2001, Lior Grossman wrote:

> Hi,
> I heard about the use of Laser Ablation for Microengineering.
> I would like to structure a material with Laser ablation method (after it
> was spinned on a Si wafer)
> and than to fill it with metal (by PVD, Electroplating, etc.).
> Do you know what is the material that I should use structuring?
> Do you know the resolution of the features that I can achieve with Laser
> Ablation?
>
>
> My Best Regards,
> Lior Grossman
> B.G. Technical Support Ltd
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
University Wafer
The Branford Group