Hi All,
I am trying to deposit 20 microns of Aluminum in Evaporation or in
Sputtering.
However, the film is very stress (more stress in sputtering).
Do you know a way to reduce the stress for such films?


My Best Regards,
Lior Grossman; Sales Manager
B.G. Technical Support Ltd (www.bg-tech.co.il)