Hi all,

I am trying to etch Lithium Niobate. I tried to etch it with buffered
HF but there is not result.

Kindly let me know if there are other etchants or techniques to etch
Lithium Niobate.

Thanks
Ashish Singh
Check out Yahoo! Shopping and Yahoo! Auctions for all of
your unique holiday gifts! Buy at http://shopping.yahoo.com
or bid at http://auctions.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Harrick Plasma, Inc.
MEMS Technology Review
Nano-Master, Inc.