A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: adhesives
adhesives
2001-12-21
kaustubh bhate
2001-12-24
Michael Yakimov
2001-12-26
Henry Yang
2002-01-14
Brubaker Chad
adhesives
Michael Yakimov
2001-12-24
        Try Aremco Crystalbond 509 (www.aremco.com ) - this is some plastic
with low melting temperature (130C), can be easily removed by acetone or by
hot photoresist remover (we use Shippley 1165 for debonding and cleanning at
the same time). We had no problems with either acids or bases treatment of
bonded substrates.
        see http://www.aremco.com/a9.html for process details
        Mike

> -----Original Message-----
> From: kaustubh bhate [SMTP:[email protected]]
> Sent: Friday, December 21, 2001 12:24 PM
> To:   [email protected]
> Subject:      [mems-talk] adhesives
>
> Hi Everybody,
> I am trying to bond some pre-thinned wafers (200um
> thick) with LPCVD nitride on it (1000A) - to a normal
> wafer substrate(500um ) thick.I need a temporary
> bonding adhesive which I should be able to remove
> after I have done some etching/lithography steps on
> the pre-thinned wafers.
>
> Does anybody know of commercially available adhesives
> that I can use for this? I need an adhesive which is
> very  simple in it's application and ideally would
> like something which I can just apply in-between the
> two wafers and then stick them together and later
> should be able to de-bond them easily too.
>
> Kaustubh Bhate.
>
> =====
> Check out Yahoo! Shopping and Yahoo! Auctions for all of
> your unique holiday gifts! Buy at http://shopping.yahoo.com
> or bid at http://auctions.yahoo.com
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Nano-Master, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics