MEMSnet Home: MEMS-Talk: Re: FW: [mems-talk] Non-Chromium Trioxide Defect Etch
Re: FW: [mems-talk] Non-Chromium Trioxide Defect Etch
2002-01-10
Victor Lifton
RE: FW: [mems-talk] Non-Chromium Trioxide Defect Etch
2002-01-10
Art Glidden
Re: FW: [mems-talk] Non-Chromium Trioxide Defect Etch
Victor Lifton
2002-01-10
Would you please send me a reference to that MEMC
paper.
Thank you,
VL

> -----Original Message-----
> From: [email protected]
> [mailto:[email protected]]On
> Behalf Of Art Glidden
> Sent: Thursday, January 10, 2002 8:20 AM
> To: [email protected]
> Subject: [mems-talk] Non-Chromium Trioxide Defect
> Etch
>
>
> Looking for a non-CrO3 etch for finding dislocation,
> slip, and stacking
> fault defects in 100 Si slices. I've read a 1990
> paper on an etch employing
> Copper Nitrate, developed at MEMC. Experience using
> that, or other, more
> user-friendly etchant for this purpose?
>
> A.G.
> _______________________________________________
> [email protected] mailing list: to unsubscribe
> or change your list
> options, visit
>
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS
> processing services.
> Visit us at http://www.mems-exchange.org/
Send FREE video emails in Yahoo! Mail!
http://promo.yahoo.com/videomail/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
The Branford Group