I recently processed a wafer and mistakenly used the wrong mask at a
certain step.  After removing the photoresist, I noticed that the areas
which had been developed were hydrophillic and the areas which had been
covered with resist were hydrophobic.  I don't know how long the effect
lasts, but I dipped the wafer in water and dried it about 5 times and the
effect remained.
Conditions were AZ 351 developer and AZ positive resist on GaAs (with some
epitaxial stuff on top).

Marty

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Addison Engineering
Process Variations in Microsystems Manufacturing
MEMStaff Inc.