MEMSnet Home: MEMS-Talk: AZ4620 problems
AZ4620 problems
2002-01-15
Alok Paranjpye
2002-01-15
Hanqing Li
2002-01-15
Charles Lakeman
2002-01-15
[email protected]
2002-01-16
Liz Shelley
2002-01-16
Danny Hirdes
2002-01-16
Islam Rafiqul
AZ4620 problems
Charles Lakeman
2002-01-15
The streaks may well be due to differential solvent evaporation rates (see
D.P. Birnie, J. Mater. Res. 16 (4), 1145, (2001)).  For thick PR coatings
try using SU-8 from Microchem Corp.  They produce resists that can generate
thick coats up to 200 microns.

Charles Lakeman,
TPL Inc.
Albuquerque, NM


----- Original Message -----
From: "Alok Paranjpye" 
To: 
Sent: Tuesday, January 15, 2002 2:47 PM
Subject: [mems-talk] AZ4620 problems


> I have a requirement for a thick (~6+ um) positive resist layer. I've been
> trying to use AZ4620 at 4000 rpm for this purpose, but it always gives me
> an uneven, streaky coating, with the streaks running in the  radial
> direction on the wafer. I have tried ramping the spin rate to avoid this,
> but the streaks remain. If anybody has had a similar experience, and could
> help me out, it would be great. Alternately, I'd appreciate any
> suggestions for another resist that could give me a thick coat, and could
> be exposed on an i-line stepper.
> Thanks
> Alok Paranjpye
>
> Graduate Student
> University of California,
> Santa Barbara
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
The Branford Group
Addison Engineering
Mentor Graphics Corporation