Porous silicon formation simulation
Luiz Marangoni
2002-01-17
>can any body give me some help about the formation of Porous Silicon.
>i am specially interested in the Pore Thickness Formation specillay the
>bahavior of current density on it. does any body know if there is a software
>tool for the
>simulation of current lines in the porous silicon.

Hi Fahak,

I have interest in porous silicon, too. I will begin my phD research in
this semester, and in a preliminar search about this subject I didn4t found
any simulation tool to porous silicon. I found a lot of models, but
simulation tool, none...
What are your interestes concerning porous silicon? I4m interest in develop
tecnologies to use (macro)Porous silicon as structural material in MEMS
devices as a way to reduce the inertial mass of the devices.

Best regards,
Luiz marangoni
[email protected]


----------
Luiz Claudio Marangoni de Oliveira
PhD Student - MEMS Enginneering
UNICAMP - State University of Campinas - Brazil

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Mentor Graphics Corporation