MEMSnet Home: MEMS-Talk: very uniform surface of elctroplated Nickel ?
very uniform surface of elctroplated Nickel ?
2002-01-19
sou zou
2002-01-22
Patrick Cheung
2002-01-21
Igor Kadija
2002-01-21
Vladimir Gelfandbein
RE: Need 3" Si wafers
2002-01-22
Qifa Zhou
2002-01-23
Kenneth Smith
2002-01-23
Mike Mattes
very uniform surface of elctroplated Nickel ?
sou zou
2002-01-19
Hi folks !

I am looking for some advices to get a very uniform surface of nickel
electroplated layers (especially on silicon). Through my bibliography research,
it seems that the trick is mainly to get an uniform current density across the
coated surface (parallel current lines). The problem is the resist pattern wich
does'nt allow to obtain that kind of strictly vertical current lines. Does
anyone has an ingenious idea or a good web address to help me overcoming such a
problem, please ?

Thank you in advance,

sz



---------------------------------
Yahoo! Courrier -- Une adresse @yahoo.fr gratuite et en frangais !

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation