metal resistant to HCl:HNO3
Liz Shelley
2002-01-24
I believe Titanium Does not etch in HCl: HNO3

> From: "Rivas, Isabel" 
> Reply-To: [email protected]
> Date: Thu, 24 Jan 2002 17:26:18 +0100
> To: "'[email protected]'" 
> Subject: [mems-talk] metal resistant to HCl:HNO3
>
> Hello,
>
> Could anyone tell me a metal which resists this etchant: HCl:HNO3 (8:1)?
>
> Thank you very much
>
> Isabel.
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
MEMS Technology Review
Tanner EDA by Mentor Graphics