[Q] Mask for isotropic silicon wet etch? (fwd)
[Q] Mask for isotropic silicon wet etch? (fwd)
2002-02-01
Zigurts Majumdar
[Q] Mask for isotropic silicon wet etch? (fwd)
2002-02-03
Roger Brennan
[Q] Mask for isotropic silicon wet etch? (fwd)
2002-02-04
[email protected]
[mems-talk] [Q] Mask for isotropic silicon wet etch? (fwd)
2002-02-12
Weili Liu
Re: Re[2]: [mems-talk] [Q] Mask for isotropic silicon wet etch?
2002-02-13
JAMES.R.THORPE
[Q] Mask for isotropic silicon wet etch? (fwd)
Zigurts Majumdar
2002-02-01
Hi,

I am trying to isotropically wet etch silicon using a 126:60:5 HNO3:H20:NH4F
etchant (as described by Williams and Muller, J. of MEMS 1996).  The etchant
appears to work well, but masks made of AZ5214 do not.  In less than
15 minutes, the AZ5214 layer has visibly thinned and formed holes.

Can anyone recommend a more durable mask (PR, metal, both or otherwise) for
this etchant?

Thanks!

Ziggy

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Tanner EDA by Mentor Graphics
The Branford Group